Influence of Aluminosilicate Clay Nanofiller Reinforcement on the Flexural Strength, Surface Hardness, Surface Roughness and Microstructure of Auto-Polymerized PMMA Denture Base Resin: An In Vitro Study

Hasanen Ali AlNamel, Ali Mohammad Ali Aljafery, Mohammed Hussein M. Alsharbaty, Mohammed A. Alsmael, Sabreen Waleed Ibrahim, Manar E. Al-Samaray

Dentistry Journal · 2026-11-09 · 14 (11) · 731

DOI: 10.3390/dj14110731 ↗
AbstractBibliografische Angaben

Abstract

Background/Objectives: Auto-polymerized polymethyl methacrylate (PMMA) is widely used in denture repair, relining, and base-plate fabrication but is susceptible to fracture due to limited flexural strength and fatigue resistance. This in vitro study investigated the concentration-dependent effects of synthetic aluminosilicate clay (ASC) nanoparticles on the flexural strength, Vickers hardness, surface roughness, and microstructure of auto-polymerized PMMA. Methods: A total of 120 specimens of SR Triplex Cold were prepared with 0 (control), 1, 3, or 5 wt.% ASC (50–100 nm; n = 30/group). ASC was dispersed in the monomer by probe sonication for 10 min. After pressure curing and storage in distilled water at 37 °C for 7 days, flexural strength, Vickers hardness, and surface roughness (Ra) were measured (n = 10/test/group). Microstructural characterization employed SEM, EDX, and XRD. Data were analyzed using ANOVA with appropriate post hoc tests (α = 0.05). Results: ASC concentration significantly affected all three properties (p < 0.001). At 1 wt.% ASC, flexural strength increased from 61.50 ± 3.37 to 79.70 ± 2.11 MPa (+29.6%), and hardness increased from 84.39 ± 3.81 to 97.84 ± 2.56 VHN. At 3 and 5 wt.%, these properties declined to 52.60 ± 3.75 and 31.70 ± 2.83 MPa, and to 63.97 ± 2.94 and 27.73 ± 2.62 VHN, respectively. Surface roughness increased with ASC concentration, from 0.102 ± 0.012 µm (control) to 0.195 ± 0.013, 0.245 ± 0.022, and 0.327 ± 0.035 µm at 1, 3, and 5 wt.%, respectively. SEM revealed favorable particle dispersion, crack deflection, and particle bridging at 1 wt.%, whereas higher concentrations promoted agglomeration, microvoid formation, and interfacial debonding. XRD confirmed the coexistence of the amorphous PMMA phase and crystalline aluminosilicate reflections. Conclusions: Under the conditions tested, 1 wt.% ASC provided the most favorable balance of mechanical and surface properties, improving flexural strength and hardness while maintaining Ra below 0.2 µm. Higher concentrations compromised mechanical performance, with the 3 and 5 wt.% groups falling below the minimum flexural strength for Type 2 polymers. The findings suggest that reinforcement depends primarily on particle dispersion and interfacial stress transfer rather than chemical modification of the PMMA backbone.

Wissen, das zu Ihrer Arbeit passt.

Vom kostenlosen Einstieg über die persönliche Recherche bis zur vollständigen Research Suite.

Tarife ansehen →

Sind alle Verlagsvolltexte enthalten?

Nein. Bibliografische Nachweise, Abstracts und Volltexte sind unterschiedliche Inhalte. Ob ein Volltext verfügbar ist, hängt von der Quelle, Open Access und Ihren vorhandenen Lizenzen ab. Ein EUVIMED-Tarif ersetzt keine zusätzlichen Verlagsrechte.

Tarife ansehen →