Adhesive Bond Durability of Resin-Matrix CAD/CAM Materials Following Different Artificial Aging Protocols
Operative Dentistry · 2026-09 · 51 (5) · 441-454
DOI: 10.2341/25-196-l ↗Abstract
ABSTRACT Purpose: The long-term clinical performance of resin-matrix CAD/CAM restorations depends on adhesive bond stability to resin cements under intraoral stresses. However, the impact of simulated aging on bond durability remains insufficiently defined. This study examined how various artificial aging protocols influence the bonding between resin-matrix CAD/CAM materials and resin cements. Methods: Two nanoceramic resins (NCRs) (Cerasmart [GC Europe, Leuven, Belgium] and Lava Ultimate [Solventum, St. Paul, MN, USA]) and one polymer-infiltrated ceramic network (PICN) material (VITA Enamic [VITA Zahnfabrik, Bad Säckingen, Germany]) were bonded to resin composites according to the manufacturers’ instructions and then subjected to six conditions: control (no aging), water storage, HCl exposure, autoclave treatment, thermal cycling, and cyclic loading. A total of 90 blocks were prepared, and 26 beam specimens were obtained from each block for microtensile bond strength (μTBS) testing. To account for clustering of beams within blocks, generalized estimating equations (GEE) were used, and a gamma distribution with a log link function was applied for μTBS data. The failure modes were analyzed using binomial GEE models. Surface morphologies were also analyzed. Results: A significant interaction between material and aging condition was found ( p = 0.001). Within the autoclave treatment group, Cerasmart exhibited significantly higher μTBS than both Lava Ultimate ( p < 0.001) and VITA Enamic ( p = 0.007), while no significant difference was observed between the latter two materials ( p = 0.929). Failure mode distribution was not significantly influenced by material type or aging condition (all p ≥ 0.098). Conclusions: The durability of bonds to resin-matrix CAD/CAM materials is primarily influenced by material composition rather than aging condition. Among the evaluated materials, Cerasmart demonstrated superior performance under autoclave aging, while failure mechanisms remained consistent across groups.
EUVIMED