Fachartikel in der Zeitschrift Journal of Esthetic and Restorative Dentistry, online erschienen am 29.10.2026. Verfasst von Luana de Melo Soares und 7 weiteren Autor:innen. Beteiligte Einrichtung: Department of Restorative Dentistry, Piracicaba Dental School, University of Campinas, Piracicaba, São Paulo, Brazil. Die Arbeit nennt 47 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: São Paulo State Research Foundation.
Abstract (Originalsprache)
Objectives
This study evaluated the effects of resin‐based materials on crack occurrence in ceramic laminate veneers (CLVs) after adhesive cementation. Additionally, the polymerization shrinkage stress (PSS) and maximum polymerization rate (MPR) of the resin‐based materials were determined. Materials and Methods Four resin‐based materials were used as luting agents: Variolink Esthetic LC (Ivoclar), SDR Plus (Dentsply), heated Z100 (69°C, Solventum), and heated VisCalor Bulk (65°C, Voco). Twenty‐eight prepared premolars received CLVs ( n = 7). CLV integrity was assessed by transillumination and scanning electron microscopy. PSS was measured in a universal testing machine and MPR by FTIR spectroscopy ( n = 5). Data were analyzed by one‐way ANOVA and Tukey's test ( α = 0.05).
Results
No CLV cracks were detected. VisCalor Bulk showed the lowest PSS (74.2 ± 15.3 MPa) and Variolink Esthetic LC the highest (135.4 ± 8.4 MPa) and the highest MPR (15.5%/s ± 2.3%/s). SDR Plus presented the lowest (10.0%/s ± 1.2%/s).
Conclusions
The type of luting agent did not influence crack formation in CLVs. The PSS and MPR varied among materials.
Schlagwörter
Stichwörter der Autor:innen
Autor:innen und Institutionen
- Department of Restorative Dentistry, Piracicaba Dental School, University of Campinas, Piracicaba, São Paulo, Brazil.
- Department of Dentistry, College of Health Sciences, Albert Einstein Israelite Brazilian Charitable Society, São Paulo, São Paulo, Brazil.
- Department of Biomaterials and Oral Biology, Faculty of Dentistry, University of São Paulo, São Paulo, São Paulo, Brazil.
- Department of Restorative Sciences, Dental College of Georgia, Augusta University, Augusta, Georgia, USA.
- Department of Molecular Pathobiology, College of Dentistry, New York University, New York City, New York, USA.
ORCID-Profile: Luana de Melo Soares, Vitaliano Gomes de Araújo-Neto, Daniel Kenji Funabashi, Bruna Marin Fronza, Roberto Ruggiero Braga, Frederick Allen Rueggeberg, Ronaldo Hirata, Marcelo Giannini
Förderung
- São Paulo State Research Foundation
Zitieren
APA
de Melo Soares, L., de Araújo-Neto, V. G., Funabashi, D. K., Fronza, B. M., Braga, R. R., Rueggeberg, F. A., Hirata, R., & Giannini, M. (2026). Evaluation of the Integrity of Ceramic Laminates After Adhesive Cementation. Journal of Esthetic and Restorative Dentistry. https://doi.org/10.1111/jerd.70292
Vancouver
de Melo Soares L, de Araújo-Neto VG, Funabashi DK, Fronza BM, Braga RR, Rueggeberg FA, et al. Evaluation of the Integrity of Ceramic Laminates After Adhesive Cementation. Journal of Esthetic and Restorative Dentistry. 2026. doi:10.1111/jerd.70292
BibTeX
@article{deMeloSoares2026,
author = {de Melo Soares, Luana and de Araújo-Neto, Vitaliano Gomes and Funabashi, Daniel Kenji and Fronza, Bruna Marin and Braga, Roberto Ruggiero and Rueggeberg, Frederick Allen and Hirata, Ronaldo and Giannini, Marcelo},
title = {Evaluation of the Integrity of Ceramic Laminates After Adhesive Cementation},
journal = {Journal of Esthetic and Restorative Dentistry},
year = {2026},
doi = {10.1111/jerd.70292}
}
EUVIMED