Fachartikel in der Zeitschrift Journal of Esthetic and Restorative Dentistry, online erschienen am 05.05.2026. Verfasst von İzim Türker Kader und 3 weiteren Autor:innen. Beteiligte Einrichtung: Department of Prosthodontics, Bahçeşehir University, School of Dental Medicine, Istanbul, Turkey. Hauptthemen laut MEDLINE: Printing, Three-Dimensional, Dental Polishing, Resins, Synthetic, Occlusal Splints. Die Arbeit wurde bisher 1-mal zitiert (Crossref) und nennt 32 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).
Abstract (Originalsprache)
Objective
The objective of this in vitro study was to evaluate the effects of different surface finishing protocols and post‐curing environments on the surface roughness (Ra) and Vickers hardness (VHN) of a 3‐dimensionally (3D)‐printed occlusal splint resin. Materials and Methods Ninety‐six disc‐shaped specimens (Ø16 × 3 mm) were fabricated from a photopolymerizable splint resin using a stereolithography 3D printer. The specimens were assigned to four surface finishing groups: as‐printed (AP), polished (P), resin‐coated (RC), and glaze‐coated (GC). Each group was further subdivided according to the post‐curing environment, air (A) or glycerin (G), resulting in eight experimental groups ( n = 12): AP‐A, AP‐G, P‐A, P‐G, RC‐A, RC‐G, GC‐A, and GC‐G. Post‐curing was performed at 60°C for 60 min. For the glycerin subgroups of the coated specimens (RC‐G and GC‐G), an initial curing period in air was applied before completing the post‐curing in glycerin to stabilize the applied coating layer. Ra was measured using a surface profilometer, and VHN was determined using a microhardness tester. The data were analyzed using two‐way ANOVA and post hoc Tukey HSD test ( α = 0.05).
Results
Surface finishing significantly affected Ra and VHN ( p < 0.001), whereas the post‐curing environment had no effect ( p > 0.05). AP‐A and AP‐G specimens showed the highest Ra, while GC‐A and GC‐G specimens exhibited the highest VHN ( p < 0.001).
Conclusions
Surface finishing is essential for optimizing surface properties of 3D‐printed occlusal splints. Although coating procedures, particularly glaze, were associated with higher surface hardness, polishing yielded smoother surfaces and provided consistent and clinically acceptable properties. Clinical Significance Surface finishing plays an important role in the clinical performance of 3D‐printed occlusal splints. Although coating procedures yield high surface hardness, polishing provides smoother, more consistent surfaces, making it a practical and reliable option for routine clinical use.
Schlagwörter
MeSH-Schlagwörter (MEDLINE)
Substanzen
Autor:innen und Institutionen
- Department of Prosthodontics, Bahçeşehir University, School of Dental Medicine, Istanbul, Turkey.
- Department of Prosthodontics, Yeditepe University, Faculty of Dentistry, Istanbul, Turkey.
- Universität Witten/Herdecke, School of Dental Medicine, Witten, Germany.
ORCID-Profile: İzim Türker Kader
Zitieren
APA
Türker Kader, İ., Karacan, E., Kursoğlu, B., & Kursoğlu, P. (2026). Effects of Polishing, Resin Coating, and Glaze Coating on the Surface Properties of a 3D ‐Printed Splint Resin. Journal of Esthetic and Restorative Dentistry, 38(9), 1814-1820. https://doi.org/10.1111/jerd.70184
Vancouver
Türker Kader İ, Karacan E, Kursoğlu B, Kursoğlu P. Effects of Polishing, Resin Coating, and Glaze Coating on the Surface Properties of a 3D ‐Printed Splint Resin. Journal of Esthetic and Restorative Dentistry. 2026;38(9):1814-1820. doi:10.1111/jerd.70184
BibTeX
@article{TrkerKader2026,
author = {Türker Kader, İzim and Karacan, Ecem and Kursoğlu, Berru and Kursoğlu, Pınar},
title = {Effects of Polishing, Resin Coating, and Glaze Coating on the Surface Properties of a 3D ‐Printed Splint Resin},
journal = {Journal of Esthetic and Restorative Dentistry},
year = {2026},
volume = {38},
number = {9},
pages = {1814--1820},
doi = {10.1111/jerd.70184}
}
EUVIMED