EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Influence of Airborne‐Particle Abrasion and Thermal Cycling on Enamel Bond Strength and Roughness of Lithium Disilicate Treated With a Self‐Etching Ceramic Primer

Gabriel Freitas Pereira iD, Maudiela Isabel Arita Torres iD, Nicole Escórcio de Meneses iD, Ana Carolina Lima Moreira iD, Raniel Fernandes Peixoto iD

Journal of Esthetic and Restorative Dentistry · 2026-07 · 38 (7) · 1367-1375

DOI: 10.1111/jerd.70132 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Journal of Esthetic and Restorative Dentistry, online erschienen am 23.02.2026. Verfasst von Gabriel Freitas Pereira und 4 weiteren Autor:innen. Beteiligte Einrichtung: Department of Restorative Dentistry, Faculty of Pharmacy, Dentistry and Nursing, Federal University of Ceará, Fortaleza, Ceará, Brazil. Hauptthemen laut MEDLINE: Dental Porcelain, Dental Enamel, Dental Bonding, Dental Etching. Die Arbeit wurde bisher 2-mal zitiert (Crossref) und nennt 56 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Objective

This in vitro study investigated the effect of a self‐etching ceramic primer (Monobond Etch & Prime [MEP]), with or without aluminum oxide airborne‐particle abrasion, on the surface roughness, and microtensile bond strength (μTBS) of lithium disilicate bonded to enamel, compared with the conventional hydrofluoric acid plus silane (HF + S). Materials and Methods Lithium disilicate specimens (10 × 10 × 4 mm) were assigned to four groups: HF + S airborne‐particle abraded (HF + S[a]), HF + S polished (HF + S[p]), MEP airborne‐particle abraded (MEP[a]), and MEP polished (MEP[p]). Surface roughness (Δ S a ) was assessed after conditioning, and specimens were bonded to bovine enamel with resin cement. μTBS was tested before and after thermo cycling (10,000 cycles, 5°C/55°C).

Results

Airborne‐particle abrasion significantly increased Δ S a (HF + S[a]: 1.16 ± 0.12 μm; MEP[a]: 0.85 ± 0.02 μm) compared to polished specimens (HF + S[p]: 0.47 ± 0.04 μm; MEP[p]: 0.38 ± 0.04 μm). HF + S and MEP performed similarly in all conditions ( p > 0.05). Airborne‐particle abraded surfaces consistently exhibited higher μTBS than polished ones ( p < 0.05). Thermo cycling significantly reduced μTBS in all groups. Mixed and cohesive failures predominated before thermo cycling, whereas adhesive failures increased after.

Conclusion

MEP and HF + S demonstrated comparable bonding to enamel. Airborne‐particle abrasion enhanced both surface roughness and μTBS, regardless of conditioning strategy. Although thermo cycling reduced adhesion in all groups, the decline was similar across treatments.

Schlagwörter

MeSH-Schlagwörter (MEDLINE)

Dental PorcelainDental EnamelDental BondingDental EtchingCeramicsSurface PropertiesAnimalsResin CementsTensile StrengthAcid Etching, DentalCattleIn Vitro TechniquesMaterials TestingAir Abrasion, Dental

Stichwörter der Autor:innen

airborne‐particle abrasiondental enamelhydrofluoric acidlithium disilicateself‐etching ceramic primer

Substanzen

Dental Porcelainlithia disilicateResin Cements

Autor:innen und Institutionen

  • Department of Restorative Dentistry, Faculty of Pharmacy, Dentistry and Nursing, Federal University of Ceará, Fortaleza, Ceará, Brazil.
  • Graduate Program in Dentistry, Federal University of Ceará, Fortaleza, Ceará, Brazil.

ORCID-Profile: Gabriel Freitas Pereira, Maudiela Isabel Arita Torres, Nicole Escórcio de Meneses, Ana Carolina Lima Moreira, Raniel Fernandes Peixoto

Zitieren

APA

Pereira, G. F., Torres, M. I. A., de Meneses, N. E., Moreira, A. C. L., & Peixoto, R. F. (2026). Influence of Airborne‐Particle Abrasion and Thermal Cycling on Enamel Bond Strength and Roughness of Lithium Disilicate Treated With a Self‐Etching Ceramic Primer. Journal of Esthetic and Restorative Dentistry, 38(7), 1367-1375. https://doi.org/10.1111/jerd.70132

Vancouver

Pereira GF, Torres MIA, de Meneses NE, Moreira ACL, Peixoto RF. Influence of Airborne‐Particle Abrasion and Thermal Cycling on Enamel Bond Strength and Roughness of Lithium Disilicate Treated With a Self‐Etching Ceramic Primer. Journal of Esthetic and Restorative Dentistry. 2026;38(7):1367-1375. doi:10.1111/jerd.70132

BibTeX
@article{Pereira2026,
  author = {Pereira, Gabriel Freitas and Torres, Maudiela Isabel Arita and de Meneses, Nicole Escórcio and Moreira, Ana Carolina Lima and Peixoto, Raniel Fernandes},
  title = {Influence of Airborne‐Particle Abrasion and Thermal Cycling on Enamel Bond Strength and Roughness of Lithium Disilicate Treated With a Self‐Etching Ceramic Primer},
  journal = {Journal of Esthetic and Restorative Dentistry},
  year = {2026},
  volume = {38},
  number = {7},
  pages = {1367--1375},
  doi = {10.1111/jerd.70132}
}
Kostenlos starten →