Influence of different immediate dentin sealing strategies on bond strength of indirect resin nanoceramic restorations
European Journal of Oral Sciences · 2024
DOI: 10.1111/eos.12983 ↗Kurz gefasst
Fachartikel in der Zeitschrift European Journal of Oral Sciences, 2024. Verfasst von Fatma-Alzahraa Mohamed Tahoun und 2 weiteren Autor:innen. Beteiligte Einrichtung: Division of Operative, Conservative Dentistry Department, Faculty of Dentistry, Alexandria University, Alexandria, Egypt. Hauptthemen laut MEDLINE: Composite Resins, Dental Bonding, Shear Strength, Resin Cements. Die Arbeit wurde bisher 4-mal zitiert (Crossref) und nennt 52 Literaturangaben.
Abstract (Originalsprache)
In this study, we evaluated the effect of four different strategies for bonding a CAD/CAM resin nanoceramic restoration (Lava Ultimate, 3M) to the dentin surface using a universal adhesive (Scotch Bond Universal, 3M) and adhesive resin cement (RelyX Ultimate, 3M) on the shear bond strength (SBS) and failure mode. The strategies comprised: (i) immediate sealing, immediate bonding; (ii) immediate sealing, bonding after 2 weeks with provisional restoration; (iii) immediate sealing with flowable resin composite reinforcement and bonding after 2 weeks with provisional restoration; and (iv) no immediate sealing, and bonding after 2 weeks with provisional restoration. After bonding, all the specimens were thermocycled, shear tests were performed using a universal testing machine, and failure modes were determined using stereomicroscope and scanning electron microscopy. The highest mean SBS was recorded with immediate sealing, immediate bonding strategy. Most adhesive failures with exposed dentinal tubules were noted in specimens exposed to bonding after 2 weeks with no immediate sealing, which was associated with the lowest SBS. Mixed failures predominated in all immediate dentin sealing groups. Immediate sealing with universal adhesives improves SBS, particularly in the single‐visit approach, which has shown significantly better performance, whereas the provisional phase has a negative effect.
Schlagwörter
MeSH-Schlagwörter (MEDLINE)
Stichwörter der Autor:innen
Substanzen
Autor:innen und Institutionen
- Division of Operative, Conservative Dentistry Department, Faculty of Dentistry, Alexandria University, Alexandria, Egypt.
ORCID-Profile: Fatma-Alzahraa Mohamed Tahoun, Hany Abdel-Ghafar Kehela, Dina Mohamed Nasr
Zitieren
APA
Tahoun, F. M., Kehela, H. A., & Nasr, D. M. (2024). Influence of different immediate dentin sealing strategies on bond strength of indirect resin nanoceramic restorations. European Journal of Oral Sciences. https://doi.org/10.1111/eos.12983
Vancouver
Tahoun FM, Kehela HA, Nasr DM. Influence of different immediate dentin sealing strategies on bond strength of indirect resin nanoceramic restorations. European Journal of Oral Sciences. 2024. doi:10.1111/eos.12983
BibTeX
@article{Tahoun2024,
author = {Tahoun, Fatma-Alzahraa Mohamed and Kehela, Hany Abdel-Ghafar and Nasr, Dina Mohamed},
title = {Influence of different immediate dentin sealing strategies on bond strength of indirect resin nanoceramic restorations},
journal = {European Journal of Oral Sciences},
year = {2024},
doi = {10.1111/eos.12983}
}
EUVIMED