Fachartikel in der Zeitschrift Dental Traumatology, 2025. Verfasst von Luiz Felipe Rodrigues Siqueira und 4 weiteren Autor:innen. Beteiligte Einrichtung: Department of Oral Rehabilitation, Federal University of Goiás, Goiânia, Goiás, Brazil. Hauptthemen laut MEDLINE: Tensile Strength, Polyvinyls, Mouth Protectors. Die Arbeit nennt 38 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Fundação de Amparo à Pesquisa do Estado de Goiás.
Abstract (Originalsprache)
Background/Aim Bi‐colored mouthguards (MTG) are often sought by both professional and amateur athletes. Bi‐colored MTG can be made in the dental office from premanufactured bi‐colored EVA sheets or custom‐designed in the dental office for greater color variety. This study aimed to evaluate the tensile strength of ethylene‐vinyl acetate (EVA) plates from two commercial brands (BioArt and Polyshok), using different bonding methods and heat sources for producing bicolored MTG. Materials and Methods EVA plates from BioArt and Polyshok (3 mm thickness) were bonded using six methods combining two bonding materials (metal angle and glass plate) and three heat sources (heat gun, mini‐torch, and Hannau lamp). Bonded plates were sectioned into 30 standardized bar‐shaped samples (70 × 10 × 3 mm) and subjected to tensile testing. Ultimate tensile strength was recorded, and statistical analyses were performed using One‐Way ANOVA and Tukey's test (α = 0.05).
Results
Significant differences in ultimate tensile strength (MPa) were observed between bonding methods ( p < 0.001) for each commercial brand. The metal angle and heat gun (MAH) method exhibited the highest tensile strength for both tested EVAs (BioArt: 146.5 ± 30 MPa; Polyshok: 87.8 ± 19.3 MPa). The Hannau lamp produced the lowest values for both tested EVAs (BioArt: 69.8 ± 43.1 MPa; Polyshok: 51.0 ± 14.4 MPa).
Conclusions
The bonding method significantly affects the tensile strength of EVA plates, with the MAH method and heat gun demonstrating superior performance. These findings highlight the importance of optimizing bonding techniques to ensure durability and protective performance in bi‐colored MTG.
Schlagwörter
MeSH-Schlagwörter (MEDLINE)
Stichwörter der Autor:innen
Substanzen
Autor:innen und Institutionen
- Department of Oral Rehabilitation, Federal University of Goiás, Goiânia, Goiás, Brazil.
ORCID-Profile: Luiz Felipe Rodrigues Siqueira, Ângelo Caetano Rodrigues Mathias Pereira, Bruno Felipe Fernandes, Leon Fernando Marques Jaime, Crisnicaw Veríssimo
Förderung
- Fundação de Amparo à Pesquisa do Estado de Goiás
Zitieren
APA
Siqueira, L. F. R., Pereira, Â. C. R. M., Fernandes, B. F., Jaime, L. F. M., & Veríssimo, C. (2025). Ultimate Tensile Strength Evaluation of Bi‐Colored Ethylene‐Vinyl Acetate (EVA) Sheets In‐Office Manufactured With Different Heating Protocols. Dental Traumatology. https://doi.org/10.1111/edt.70036
Vancouver
Siqueira LFR, Pereira ÂCRM, Fernandes BF, Jaime LFM, Veríssimo C. Ultimate Tensile Strength Evaluation of Bi‐Colored Ethylene‐Vinyl Acetate (EVA) Sheets In‐Office Manufactured With Different Heating Protocols. Dental Traumatology. 2025. doi:10.1111/edt.70036
BibTeX
@article{Siqueira2025,
author = {Siqueira, Luiz Felipe Rodrigues and Pereira, Ângelo Caetano Rodrigues Mathias and Fernandes, Bruno Felipe and Jaime, Leon Fernando Marques and Veríssimo, Crisnicaw},
title = {Ultimate Tensile Strength Evaluation of Bi‐Colored Ethylene‐Vinyl Acetate (EVA) Sheets In‐Office Manufactured With Different Heating Protocols},
journal = {Dental Traumatology},
year = {2025},
doi = {10.1111/edt.70036}
}
EUVIMED