Building Pores from Thin Air: Nanobubble-Treated Catalyst Inks Improve Catalyst Utilization and Durability in PEM Water Electrolyzer Anodes
ACS Applied Energy Materials · 11.11.2026
DOI: 10.1021/acsaem.6c02654 ↗Kurz gefasst
Fachartikel in der Zeitschrift ACS Applied Energy Materials, online erschienen am 11.11.2026. Verfasst von Mohamed E. Abdelrahman und 3 weiteren Autor:innen. Die Arbeit nennt 70 Literaturangaben. Gefördert von: Moleaer Inc..
Abstract (Originalsprache)
The architecture of the anode catalyst layer is set at the ink stage, yet few ink-level tools exist to engineer that architecture. Here, we introduce bulk air nanobubbles (NBs; 95–118 nm mean diameter, 280–1340 × 106 mL–1) into the water phase of IrOx anode inks in proton exchange membrane water electrolyzers (PEMWEs) to disperse the ink solids more finely and to template additional porosity into the resulting catalyst layer. In a five-level concentration screen, the two lowest NB concentrations outperformed the baseline and the three higher concentrations performed within a few percent of it. The best electrode, made at the lowest NB concentration, showed +16.3% higher current density at 2.0 V (+22.5% Ir-mass-normalized), +41% higher Ir-mass activity at 1.46 V, similar Tafel slopes, 10% lower high-frequency resistance, 61% higher double-layer capacitance, and 20% lower polarization resistance. Normalizing the current by the measured double-layer capacitance removes the advantage, which places the gains in accessible catalyst area rather than in intrinsic activity. FIB-SEM tomography of one volume per electrode shows a porosity of 26.2% in the treated layer against 20.5% in the baseline, a uniform hierarchical structure in place of a densified band at the PTL side, and an added pore population commensurate with the bubble size. Pore network modeling on the reconstructed volumes predicts +93% permeability and a division of roles between the two pore populations: drained large pores evacuate oxygen while fine pores immobilize water, retaining 19% more membrane-side saturation at operating capillary pressures. Electrochemical ionomer-coverage measurements, applied to a PEMWE anode for the first time, rise from 92.2 to 98.0%. Together with a 15% gain in catalyst-pore interfacial area per unit catalyst volume, this is consistent with a treatment that disperses both the catalyst and the ionomer more effectively. In a 144 h square-wave accelerated stress test on one electrode of each type, the NB-treated electrode degraded less (7.9% versus 10.2% at 2.2 V), its polarization-resistance growth was nearly halved, and post-mortem μ-XRF showed less spatially correlated iridium redistribution. Nanobubble treatment is a solvent-side change that leaves the ink composition and the coating process untouched.
Förderung
- Moleaer Inc.
Zitieren
APA
Abdelrahman, M. E., Tolouei, N. E., Zenyuk, I. V., & Akhter, S. (2026). Building Pores from Thin Air: Nanobubble-Treated Catalyst Inks Improve Catalyst Utilization and Durability in PEM Water Electrolyzer Anodes. ACS Applied Energy Materials. https://doi.org/10.1021/acsaem.6c02654
Vancouver
Abdelrahman ME, Tolouei NE, Zenyuk IV, Akhter S. Building Pores from Thin Air: Nanobubble-Treated Catalyst Inks Improve Catalyst Utilization and Durability in PEM Water Electrolyzer Anodes. ACS Applied Energy Materials. 2026. doi:10.1021/acsaem.6c02654
BibTeX
@article{Abdelrahman2026,
author = {Abdelrahman, Mohamed E. and Tolouei, Nadia E. and Zenyuk, Iryna V. and Akhter, Sohail},
title = {Building Pores from Thin Air: Nanobubble-Treated Catalyst Inks Improve Catalyst Utilization and Durability in PEM Water Electrolyzer Anodes},
journal = {ACS Applied Energy Materials},
year = {2026},
doi = {10.1021/acsaem.6c02654}
}
EUVIMED